Rubber Coated Stainless Steel, 4 1/2 lb. Roller (75 A ± 5 Scale)
- DESCRIPTION
- DATA SHEET
- ACCESSORIES
-
Rubber coated stainless steel, 4 1/2 lb. Roller, 75 A ±5 scale (Certificate not included, add item 107412591 for certification)
This method covers a suitable procedure for establishing the acceptability of interlayer and surface adhesion of a water-immersed organic coating system. The procedure can be used as a production test.
4-1/2 pound rubber covered roller that has a surface durometer hardness value within the range of 70 to 80. The roller is approximately 3-1/2" in diameter and 1-3/4" wide. It is made of steel and has two plastic handles.
Instructions for use
Apply the coating system to the substrate and allow to dry as specified in the product specification. Immerse the test sample in distilled water for 24 hours. Remove the test sample from the water and dry it with a soft cloth. Within 1 minute of removing it from the water, make two parallel scratches, about an inch apart, across the coating to the metal with a stylus.
See Scriber below.) Immediately apply a 1" wide strip of the masking tape sticky side down across the scratches. Press the tape against the coating surface by rolling the roller across the tape eight times. Remove the tape with a Move quickly and examine for damage to the intercoat or surface adhesion. Store the roller using the supplied acrylic ring holder, this prevents the rubber mat from being crushed. -
Technical data of the standards Rules: ASTM D2510, D1000, D3330, D3330M, D1654, BSS7225 / Federal Standard Test Method 141D and 141C Method 6301.2 and 6301.3 / MIL-PRF-23377, MIL-PRF-85285, A2TS 4860, BATS 4860 see specific articles below PA-1411: Meets federal test standards 141D and 141C, M6301.2, M6301.3, MIL-PRF-23377, MIL-PRF-85285, MIL-PRF-81352C, MIL-C-5541E, A2TS 4860, BATS 4860 PA-1431: Meets ASTM D2510, D1000, D3330, D3330M, BSS7225 standards PA-142011: ASTM D2510 SL-5010 : ASTM B117, A1.2.1, ASTM D1654
What includes:
*Acrylic ring holder.